Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 160 - 200 °C | 320 - 392 °F | |
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Maximum Service Temperature, Air | 130 - 200 °C | 266 - 392 °F | Average value: 143 °C Grade Count:12 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Maximum Service Temperature, Air | 120 - 200 °C | 248 - 392 °F | Average value: 153 °C Grade Count:7 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Maximum Service Temperature, Air | 170 - 200 °C | 338 - 392 °F | Average value: 189 °C Grade Count:7 |
Overview of materials for Phenolic, Novolac, Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Maximum Service Temperature, Air | 80.0 - 200 °C | 176 - 392 °F | Average value: 140 °C Grade Count:10 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Maximum Service Temperature, Air | 80.0 - 200 °C | 176 - 392 °F | Average value: 124 °C Grade Count:8 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Maximum Service Temperature, Air | 80.0 - 200 °C | 176 - 392 °F | Average value: 128 °C Grade Count:4 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Maximum Service Temperature, Air | -60.0 - 200 °C | -76.0 - 392 °F | |
SMAC BARRIER® Damping Material SMAC BARRIER® is a new material developed by SMAC to complete the range of solutions for noise reduction into an aircraft. SMAC BARRIER® is an acoustic layer designed to reduce the transmissio.. |
|||
Maximum Service Temperature, Air | 150 - 200 °C | 302 - 392 °F | |
Goodfellow Polyvinyl Fluoride (PVF) Film A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v.. |
|||
Maximum Service Temperature, Air | 180 - 200 °C | 356 - 392 °F | Average value: 189 °C Grade Count:9 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Maximum Service Temperature, Air | 180 - 200 °C | 356 - 392 °F | Average value: 190 °C Grade Count:4 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Maximum Service Temperature, Air | 80.0 - 200 °C | 176 - 392 °F | Average value: 123 °C Grade Count:6 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Maximum Service Temperature, Air | 75.0 - 200 °C | 167 - 392 °F | Average value: 132 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |