Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 491 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 255 °C
491 °F
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
Maximum Service Temperature, Air 255 °C
491 °F
Lehmann & Voss LUVOCOM® 1104-8327 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts.Low warpage.Information pro..
Maximum Service Temperature, Air 255 °C
491 °F
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
Maximum Service Temperature, Air 255 °C
491 °F
Deflection Temp at unknown load
Abatron AboCast 8501-6 One-Component Epoxy
AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E..