Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 188 - 210 °C | 370 - 410 °F | Average value: 200 °C Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | Heat resistance per ASTM D794 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | Heat Resistance; ASTM D570D |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | Heat Resistance; ASTM D570D |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | Heat Resistance; ASTM D570D |
Plenco 7080 Phenolic, Nodular, Compression Molded PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de.. |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | Heat Resistance; ASTM D570D |
Plenco 7203 Phenolic, Granular, Transfer Molded PLENCO 07203 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and an industrial finish. UL recognized under component file E40654. 07203 is available i.. |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | See Note 2. |
ChevronTexaco Crater® 2X Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Maximum Service Temperature, Air | 188 °C | 370 °F | Heat Resistance; ASTM D570D |
Plenco 6527 Phenolic, Granular, Injection Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |