Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 149 °C | 300 °F | Intermittent |
Plasma Coatings 800-N Surface Material Information provided by Plasma Coatings |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Ritelok GM15 General Purpose Gasket Maker Anaerobic. General -purpose gasket maker for housings, flanges, and pipework. Replaces pre-cut gaskets, Does not shrink or relax, flexible, Withstands temperatures from 65°F to 300°F (5.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
ND Industries 150 Wicking Adhesive High Pressure Sealant Seals pores in welds and hairline cracks in castings |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
ND Industries 541 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, cams, collars, flywheels, rotors to shaft |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
ND Industries NutGrade® 121 Removable Threadlocker A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Permabond HM129 Anaerobic Threadlocker Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Master Bond UV10TKLO-2 UV Curable Compound for Aerospace Applications Description: Master Bond UV10TKLO-2 is a special one component UV curable epoxy modified system for high performance bonding, sealing and encapsulation. This system has passed rigorous testing to me.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Master Bond UV15 High Strength UV Curable Adhesive System Master Bond UV15 is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is al.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Heat Resistance; ASTM D570D |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 3493 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 3526 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 392 Rapid Fixture Structural Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 5205 Flexible Cure Flange Sealant Anaerobic GasketingLoctite® 5205 Flexible Cure Flange SealantFast curing and flexible, good sealing properties against oil and water/glycol particularly at high temperatures. High viscosity. Recom.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 641 Controlled Strength Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® Gasket Eliminator® 518 Flange Sealant Anaerobic GasketingLoctite® 518 Flexible Cure Gasket Eliminator® Flange SealantForms a flexible, solvent-resistance seal that will not tear or decay. Seals to 300ºF and fills gaps to 0.050". Can.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
ChevronTexaco FM NLGI 0 Grease EP FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greas.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Operating Temperature |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | intermittent |
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM) Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Short term |
3M 4412G Extreme Sealing Tape 3M™ Extreme Sealing Tape is a family of single coated, pressure sensitive adhesive tapes designed for difficult sealing applications. The backing on this tape is an ionomer film that is very tough .. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | up to 30 mins |
3M 2497ST High-Temperature Tear Resistant Polyester Tape 3M™ High-Temperature Tear Resistant Polyester Tape 2497ST is designed for use in masking applications where sliver resistance and clean removal are required.Information provided by 3M |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Service |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M 8411 Edging and Reinforcing Tape 3M™ Edging and Reinforcing Tape 8411 is a transparent polyester film tape for many permanent edging and reinforcing types of applications.Information provided by 3M |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M Scotch® 2517 Flatback Tape Scotch® Flatback Tape 2517 is a general purpose tape for splicing liner boards, bundling, holding packing applications.Information provided by 3M |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M 1003 SL Fire Barrier Water Tight Sealants 3M Fire Barrier Water Tight Sealants 1000 NS and 1003 SL are ready-to-use, single component, neutral cure, silicone sealants that cure upon exposure to atmospheric humidity to form a flexible firest.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
3M Scotch-Weld™ RT35 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | Temperature Index |
AlphaGary Megolon™ S530 Low Smoke Halogen Free Highly flexible sheathing grade with a low Young's Modulus and excellent fire retardancy. Application example includes Radio Frequency. |
|||
Maximum Service Temperature, Air | 149 °C | 300 °F | |
Loctite® 511 Fast Curing Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |