Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Pyrotek Pyroboard™ S1200 Roller Pyroboard™ S1200 is a long wearing durable, soft covering. It must be used in high heat areas in order for it to realize its full effectiveness. The heat helps to sinter the materials so that the.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast CURON 120 C Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast C Sp Dense Refractory Brick Description: A fireclay brick for use up to 1200°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics ZAP 010 Smart Cast Application Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics Sharada LTM 0.5 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sapco C 221 Steatite Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
CeramTec V 38 Alumina, 96.0% Al2O3-SiO2 Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-DA Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-DM Refractory Sheet TYPE RS-DM Sheet is a moldable form of Type RS-D with a higher density than obtainable from Refractory Sheet Type RS-DA. Type RS-DM is ideally suited for fabricating complex shapes from a flat sheet.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-DR Refractory Sheet TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-SI SILICA MOLDABLE ZIRCAR Silica Moldable Type RS-SI Moldable is a wet blanket that is a combination of high purity amorphous silica fibers and inorganic silica binder. The fibers are 6-9 um in diameter and are consid.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories APC-120 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories DC-2BS Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories GUN-120L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1200 °C | >= 2190 °F | |
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics) LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is.. |
|||
Maximum Service Temperature, Air | >= 1200 °C | >= 2190 °F | |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve component.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics 0.4 Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |