Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sharadaa Ceramics ZAP 010 Smart Cast Application

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name ZAP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics ZAP 010 Smart Cast Application.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Special Properties: High Strength CastableIndustry: Non-FerrousApplication: Aluminum Melting/Holding FurnaceInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.90 g/cc
>= 0.105 lb/in³
After Drying at 110°C
Grain Size <= 10000 µm
<= 10000 µm
Mechanical Properties Metric English Comments
Compressive Strength 93.2 MPa

@Temperature 110 °C
13500 psi

@Temperature 230 °F
Cold Crushing
101 MPa

@Temperature 1200 °C
14700 psi

@Temperature 2190 °F
Cold Crushing
142 MPa

@Temperature 1100 °C
20600 psi

@Temperature 2010 °F
Cold Crushing
58.8 MPa

@Time 86400 sec
8530 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1200 °C
2190 °F
Descriptive Properties Value Comments
Refractoriness >1500°C
Thermal Expansion 0.9
@ 1000°C, Reversible
Water Required to Mix 10-12%