Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Continuous; FRISETTA Test Method |
Nilit RECONYL B KV30 Recycled nylon 6 for injection molding, 30% glass ball reinforced Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Heat Distortion Temp |
Lucky IH-830 Acrylic, Injection Grade Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent.. |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Deflection Temp; Load not reported; ASTM D648 |
Lucky IH-830 Acrylic, Injection Grade Similar to grade EH-910, but with higher flow for injection molding. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent.. |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Deflection Temp; Load not reported; ASTM D648 |
Lucky CH-910 Acrylic, Coextrusion Grade Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Heat Distortion Temp |
Lucky CH-910 Acrylic, Coextrusion Grade Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Maximum Service Temperature, Air | 98.0 - 300 °C | 208 - 572 °F | Average value: 227 °C Grade Count:6 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Deflection Temp; Load not specified; ASTM D648 |
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
(discontinued **) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Heat Distortion Temp |
Lucky EH-910 Acrylic, Extrusion Grade Highest heat and stress cracking resistance of Lucky PMMA grades. Recommended for extrusion of sheets, pipes, and profiles. Can also be used for injection molding of small parts. May be UV stabil.. |
|||
Maximum Service Temperature, Air | 98.0 °C | 208 °F | Deflection Temp; Load not reported; ASTM D648 |
Lucky EH-910 Acrylic, Extrusion Grade Highest heat and stress cracking resistance of Lucky PMMA grades. Recommended for extrusion of sheets, pipes, and profiles. Can also be used for injection molding of small parts. May be UV stabil.. |