Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable 0800-xx01D Polyvinyl Chloride, Flexible (PVC, Flexible) NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable W2407L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 60.0 - 80.0 °C | 140 - 176 °F | Average value: 65.0 °C Grade Count:4 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Maximum Service Temperature, Air | 60.0 - 85.0 °C | 140 - 185 °F | Average value: 66.3 °C Grade Count:4 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Lushan L-5R Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Henkel Frekote 44-NC Mold Release Agent A non-CFC release agent designed to provide multiple releases with no contaminating transfer. Can be used for the release of thermoplastics, thermosetting resins, boron, aramid, graphite / carbon fi.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 4167 Polyvinyl Chloride, Flexible Notes: 60°C Jacket; RoHS Compliant Features: High Gloss; Sunlight Resistant (720 hours)Uses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW; SJT; SRDT; ST; SVT Agency Ratings: UL QM.. |
|||
Maximum Service Temperature, Air | <= 60.0 °C | <= 140 °F | Laundering Resistance |
EMS-Griltech Griltex® 1A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Maximum Service Temperature, Air | <= 60.0 °C | <= 140 °F | Laundering Resistance |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP012202 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP016902 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP024408 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products FP024402 and FP024408 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3800, which is an ultra remova.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FP10R2 Clear Polypropylene Label Product 3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV09D Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV392 Removable White Vinyl Label Products 3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive .. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FVT40 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Application |
3M FS442 Matte Clear Polystyrene Label Products 3M™ Matte Clear Polystyrene Label Products FS442 is a hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, whic.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FS501 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV010002 Removable Vinyl Label Product 3M™ Removable Vinyl Label Product FV010002 is a flexible, conformable white vinyl label stock that offers durability and moisture resistance. This vinyl label utilizes 3M™ Adhesive R3800, which is.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV034 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
AlphaGary Evoprene™ CE 6186 Thermoplastic Elastomer The Evoprene™ CE range has been specially created to offer processors a cost engineered range of easy processing, fast cycling thermoplastic elastomer compounds for general purpose applications. E.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Continuous Use; ASTM D794 |
Teknor Apex APEX® 80118-Y Polyvinyl Chloride, Flexible Notes: 60°C Insulation; RoHS Compliant Features: Good UV Resistance Uses: Cable Jacketing; InsulationAgency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire Types: TWInformation Provided.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV016402 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV016405 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | Service |
3M FV024702 White Vinyl Label Products 3M™ White Vinyl Label Products are flexible and conformable materials that offer durability and moisture resistance. The polymerically plasticized nature of this soft vinyl imparts long term dimens.. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | |
Abatron 84072 A/B Filled Potting Compound
(discontinued **) Dark gray tungsten carbide filled "carbepoxtll" abrasion resistant casting, adhesive, and resurfacing. 100/10 ratio.Information provided by Abatron. |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable 0953-xx04D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 60.0 °C | 140 °F | UL Temperature Rating |
PolyOne Geon™ Vinyl Wire & Cable JA508AF Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |