Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
Nye Lubricants UniFlor 8190 (483) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Recommended |
Nye Lubricants UniFlor 8622 (851) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S60S Silicone Rubber Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Excellent steam resistance. Formulated using only those ingredients determi.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S65G Silicone Rubber Low Compression Set, Green Silicone Rubber, 65-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Low compr.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S65T Silicone Rubber Translucent Silicone Rubber, 55-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United Sta.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S70G Silicone Rubber Green Silicone Rubber, 66-75 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated using only those ingredients determined by the United States F.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S80B Silicone Rubber Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ.Applications: Excellent heat resistance and .. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Precision Polymer Engineering S80N Silicone Rubber Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Grade .. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Silicone filled |
P & P Technology Monex Expanded Monel Foil Monex is an expanded monel foil of uniform thickness (0.5mm or 0.75mm available) which is manufactured to give a large number of contact points per cm². It can be supplied with a filler of silicon.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7301 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Möller Medical PolySkin 102 M NanoCoating Decorative, thermally stable coating with "metallic look," easy-to-clean effect can be added.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-1963 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.Chemical and hydrolysis resistance parts, non f.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Lehmann & Voss LUVOCOM® 1105-8184 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | short term; EMS |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Intermittent |
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-8 is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a higher viscos.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous use |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | DSC |
Adamas Rixon 430 PEEK, 30% Carbon Fiber Information provided by Adamas, HPM |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Maximum Service Temperature, Air | 250 °C | 482 °F | |
Beijing Evergrow Resources PTFE Porous Film The membrane is smooth, not adhesive, and wearable. It is anti impact, anti corrosive, anti high temperature and anti aging. It is also waterproof, easy to clean and has an excellent stability under.. |