Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 191 °C | 375 °F | |
Lubriplate 930-2 Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | |
Lubriplate 930-A Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | |
Lubriplate 930-AA Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | |
Lubriplate 930-AAA Bentone Type Multi-Purpose Grease Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | ASTM D1329 |
Seals Eastern 7204 Ethylene-Propylene Rubber Y267-Type EPDM for geothermal steam service. Ultra-Low compression set.Information provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 191 °C | 376 °F | |
Specialty Materials 5505 Boron Epoxy Prepreg Tape Specialty Materials' 5505 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Exhibiting exceptional performance at temp.. |
|||
Maximum Service Temperature, Air | 191 °C | 376 °F | Heat Resistance; ASTM D570D |
Plenco 2369 Phenolic, Granular, Compression Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | |
ConocoPhillips 1 HD Calcium Grease NLGI No. 1 Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusive.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | |
ConocoPhillips 2 Super Lube M EP Grease NLGI No. Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road.. |
|||
Maximum Service Temperature, Air | 191 °C | 375 °F | |
PSM Industries Ferro-TiC® C Medium Alloy Tool Steel Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.Exce.. |
|||
Maximum Service Temperature, Air | 191 °C | 376 °F | Heat Resistance; ASTM D570D |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |