Lubriplate 930-2 Bentone Type Multi-Purpose Grease

Category Fluid , Lubricant , Clay Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 930-2 Bentone Type Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short intervals up to 400°F / 204°C. Available in 4 NLGI densities for a wide range of applications. Applications: Multi-purpose, high temperatures.930 Series Greases are available in Cartridges, Tubes, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 750 SUS
750 SUS
Kinematic Viscosity at 40°C (104°F) 135 cSt
135 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 265
265
Unknown Amount of Work
Penetration P(60), 1/10 mm 295
295
Unknown Amount of Work
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 191 °C
375 °F
204 °C
400 °F
Short Intervals
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Approx. Cold test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 2
Rust/Oxidative Additives YES
Water Resistant YES