Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1200 °C | 2200 °F | |
Haynes NS-163® Cobalt Alloy Alloy that brings high-temperature alloy performance at temperatures up to 2200°F (1204°C). HAYNES NS-163 alloy is a wrought cobalt-based alloy (Co–28Cr–21Fe–9Ni–1.25Tiâ€.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2200 °F | Upper limit of working range |
Heatbath/Park Carbon Cover A specially selected graphite which can be used as a floating cover on molten neutral salt baths or as additional cover for carburizing salts. Park Carbon supplements the cover material incorporated.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Gouda Vuurvast CURON 120 S Dense Refractory Castable Description: A very strong castable with a high abrasion resistance of which both aggregate and cement attribute to hydraulic binding.Remarks: These values apply to cast products. Also available in .. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics CFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics Sharada LTM 0.4 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | exceptional strength to 1200°C |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2192 °F | |
Stellar Canada CERAMITE® BKR-S Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sharadaa Ceramics Sharada LTM 0.5 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Sapco C 220 Steatite Information provided by Sapco. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-DR Refractory Sheet TYPE RS-DR is a rigid pre-fired sheet that has been heat-treated to remove all organic binder and is stable to moisture attack. Refractory Sheet Type RS-DR is suited for use as a setter or barrier f.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Zircar Refractory Composites RS-SI SILICA MOLDABLE ZIRCAR Silica Moldable Type RS-SI Moldable is a wet blanket that is a combination of high purity amorphous silica fibers and inorganic silica binder. The fibers are 6-9 um in diameter and are consid.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories INCT-120N Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | limited |
Chosun Refractories INCT-120S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | >= 1200 °C | >= 2190 °F | |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | no load |
Accuratus Accuflect™ Light-Reflecting Ceramic Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: .. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve component.. |
|||
Maximum Service Temperature, Air | 1200 °C | 2200 °F | |
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride Fine grain aluminum nitride castable with high thermal conductivity. |
|||
Maximum Service Temperature, Air | 1200 °C | 2190 °F | |
Anderman Ceramics EZM 96 Zirconia, 96.5%, Magnesia-Stabilized Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |