Thermal Properties Metric English Comments
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy plate
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 0% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 10% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 10% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 10% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 10% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 20% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 20% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 20% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 30% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 30% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 30% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 40% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 40% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 40% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 40% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, plate, 4000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, plate, 8000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Thermal Conductivity 26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
Crucible Steel CPM® 10V® (AISI A11) Tool Steel
CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistan..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, GMAW deposit weld metal
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, plate, 1000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, plate, 16000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy plate, 16000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy plate, 8000 hours exposure at 649°C (1200°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 50% cold reduction
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 50% cold reduction, 1121°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, 50% cold reduction, 1177°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Thermal Conductivity 26.4 W/m-K

@Temperature 900 °C
183 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Copyright © lookpolymers.com All Rights Reserved