Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Crucible Steel CPM® 10V® (AISI A11) Tool Steel

Category Metal , Ferrous Metal , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Crucible Steel
Trade Name CPM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel CPM® 10V® (AISI A11) Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CPM 10V was the first in the family of high vanadium tool steels made by the Crucible Particle Metallurgy process. Crucible engineers optimized the vanadium content to provide superior wear resistance while maintaining toughness and fabrication characteristics comparable to D2 and M2. Since its introduction in 1978, CPM 10V has become recognized world-wide and sets the standard for highly wear resistant industrial tooling. Its exceptional wear resistance and good toughness make it an excellent candidate to replace carbide and other highly wear resistant materials in cold work tooling applications, particularly where tool toughness is a problem or where cost effectiveness can be demonstrated.The CPM process produces very homogeneous, high quality steel characterized by superior dimensional stability, grindability, and toughness compared to steels produced by conventional processes.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.418 g/cc
0.2680 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 255 - 277
255 - 277
Annealed
Hardness, Rockwell C 60
60
Modulus of Elasticity 221 GPa
32100 ksi
Flexural Strength 4322 MPa
626900 psi
Hardening Temperature- 1175°C, Tempering Temperature- 540°C
4377 MPa
634800 psi
Hardening Temperature- 1120°C, Tempering Temperature- 550°C
Charpy Impact 20.0 J
14.8 ft-lb
Hardening Temperature- 1175°C; Tempering Temperature- 540°C
30.0 J
22.1 ft-lb
Hardening Temperature- 1120°C; Tempering Temperature- 550°C
35.0 J
25.8 ft-lb
Hardening Temperature- 1065°C; Tempering Temperature- 550°C
Thermal Properties Metric English Comments
CTE, linear 10.7 µm/m-°C

@Temperature 21.0 - 93.0 °C
5.94 µin/in-°F

@Temperature 69.8 - 199 °F
11.1 µm/m-°C

@Temperature 21.0 - 260 °C
6.17 µin/in-°F

@Temperature 69.8 - 500 °F
12.3 µm/m-°C

@Temperature 21.0 - 593 °C
6.83 µin/in-°F

@Temperature 69.8 - 1100 °F
Thermal Conductivity 20.39 W/m-K
141.5 BTU-in/hr-ft²-°F
21.54 W/m-K

@Temperature 100 °C
149.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
24.85 W/m-K

@Temperature 300 °C
172.5 BTU-in/hr-ft²-°F

@Temperature 572 °F
26.3 W/m-K

@Temperature 500 °C
183 BTU-in/hr-ft²-°F

@Temperature 932 °F
Component Elements Properties Metric English Comments
Carbon, C 2.45 %
2.45 %
Chromium, Cr 5.25 %
5.25 %
Iron, Fe 81.25 %
81.25 %
As Remainder
Molybdenum, Mo 1.3 %
1.3 %
Vanadium, V 9.75 %
9.75 %
Users viewing this material also viewed the following: