Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco 10 WOLLASTOCOAT® Wollastonite Chemically treated grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco HARRP™ 40 Wollastonite HARRP™ 40 is suggested for concrete, roof tile, grout/stucco, etc. reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distin.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco HARRP™ Coarse Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco MD400 WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 1250 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 325 Wollastonite Powdered grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particl.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 400 Wollastonite Chemically treated powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an .. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 5000 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYAD® MG Wollastonite High aspect ratio grade. This grade is recommended for elastomer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinct.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® 12 Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® 20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 W/m-K | 18.3 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® H20-FC Electrically Conductive Epoxy Product Description: EPO-TEK®H20E-FC is a two-component, electrically conductive, snap curing epoxy for photovoltaic thin film module stringing, semiconductor packaging and PCB circuit assembly.Adv.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco 10 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Thermal Conductivity | 2.63 - 2.77 W/m-K | 18.3 - 19.2 BTU-in/hr-ft²-°F | |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |