Nyco NYGLOS® M30 Wollastonite

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nyco
Trade Name NYGLOS®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nyco NYGLOS® M30 Wollastonite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a broad range of industrial and consumer applications, including polymer reinforcement; coatings; construction/architecture reinforcement; enhancing friction stability in discs, lings, and brakes; and metallurgy.Information provided by NYCO Minerals.
Physical Properties Metric English Comments
Bulk Density 0.760 g/cc
0.0275 lb/in³
Loose
1.22 g/cc
0.0441 lb/in³
Tapped
Density 2.90 g/cc
0.105 lb/in³
Brightness 80 %
80 %
G.E. Brightness
Oil Absorption 31 %
31 %
Solubility in Water 0.0095 %
0.0095 %
Moisture Absorption 0.100 %
0.100 %
Particle Size >= 12 µm
>= 12 µm
10% smaller than
38 µm
38 µm
median; Microtrac
<= 120 µm
<= 120 µm
90% smaller than
pH 9.9
9.9
10% Slurry
Specific Surface Area 0.35 m²/g
0.35 m²/g
BET
Molecular Weight 116 g/mol
116 g/mol
Mechanical Properties Metric English Comments
Hardness, Mohs 4.5
4.5
Tensile Strength 2700 - 4100 MPa
<br>@Diameter 0.00300 - 0.150 mm
392000 - 595000 psi
<br>@Diameter 0.000118 - 0.00591 in
Fiber Strength
Modulus of Elasticity 303 - 530 GPa
<br>@Diameter 0.00300 - 0.150 mm
43900 - 76900 ksi
<br>@Diameter 0.000118 - 0.00591 in
Fiber Modulus
Thermal Properties Metric English Comments
CTE, linear 6.50 µm/m-°C
3.61 µin/in-°F
Thermal Conductivity 2.63 - 2.77 W/m-K
18.3 - 19.2 BTU-in/hr-ft²-°F
Melting Point 1410 °C
2570 °F
ASTM D1857
1540 °C
2800 °F
theoretical
Optical Properties Metric English Comments
Refractive Index 1.63
1.63
Component Elements Properties Metric English Comments
Al2O3 0.25 %
0.25 %
CaO 45.72 %
45.72 %
Fe2O3 0.25 %
0.25 %
K2O 0.20 %
0.20 %
Loss on Ignition(%) 6.3 %
6.3 %
MgO 0.71 %
0.71 %
MnO 0.020 %
0.020 %
SiO2 46.52 %
46.52 %
TiO2 0.050 %
0.050 %
Electrical Properties Metric English Comments
Electrical Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
pure wollastonite
Dielectric Constant 6.8
<br>@Frequency 10000 Hz
6.8
<br>@Frequency 10000 Hz
6.8
<br>@Frequency 100000 Hz
6.8
<br>@Frequency 100000 Hz
6.9
<br>@Frequency 1.00e+6 Hz
6.9
<br>@Frequency 1.00e+6 Hz
6.9
<br>@Frequency 1000 Hz
6.9
<br>@Frequency 1000 Hz
Dissipation Factor 0.00152
<br>@Frequency 1000 Hz
0.00152
<br>@Frequency 1000 Hz
0.0046
<br>@Frequency 10000 Hz
0.0046
<br>@Frequency 10000 Hz
0.0046
<br>@Frequency 1.00e+6 Hz
0.0046
<br>@Frequency 1.00e+6 Hz
0.0078
<br>@Frequency 100000 Hz
0.0078
<br>@Frequency 100000 Hz
Descriptive Properties Value Comments
Appearance White
Bulking Value (gal./lbs.) 0.0413
Minus 100 U.S. Mesh Screen (%) 99
Morphology Acicular