Nyco ULTRAFIBRE® 4W Wollastonite

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Nyco
Trade Name ULTRAFIBRE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Nyco ULTRAFIBRE® 4W Wollastonite.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a broad range of industrial and consumer applications, including polymer reinforcement; coatings; construction/architecture reinforcement; enhancing friction stability in discs, lings, and brakes; and metallurgy.Information provided by NYCO Minerals.
Physical Properties Metric English Comments
Bulk Density 0.200 g/cc
0.00723 lb/in³
Loose
0.350 g/cc
0.0126 lb/in³
Tapped
Density 2.90 g/cc
0.105 lb/in³
Brightness 92 %
92 %
G.E. Brightness
Oil Absorption 55 %
55 %
Solubility in Water 0.0095 %
0.0095 %
Moisture Absorption 0.100 %
0.100 %
Particle Size >= 3.0 µm
>= 3.0 µm
10% smaller than
7.0 µm
7.0 µm
median; Microtrac
<= 20 µm
<= 20 µm
90% smaller than
pH 9.9
9.9
10% Slurry
Specific Surface Area 2.9 m²/g
2.9 m²/g
BET
Molecular Weight 116 g/mol
116 g/mol
Mechanical Properties Metric English Comments
Hardness, Mohs 4.5
4.5
Tensile Strength 2700 - 4100 MPa
<br>@Diameter 0.00300 - 0.150 mm
392000 - 595000 psi
<br>@Diameter 0.000118 - 0.00591 in
Fiber Strength
Modulus of Elasticity 303 - 530 GPa
<br>@Diameter 0.00300 - 0.150 mm
43900 - 76900 ksi
<br>@Diameter 0.000118 - 0.00591 in
Fiber Modulus
Thermal Properties Metric English Comments
CTE, linear 6.50 µm/m-°C
3.61 µin/in-°F
Thermal Conductivity 2.63 - 2.77 W/m-K
18.3 - 19.2 BTU-in/hr-ft²-°F
Melting Point 1410 °C
2570 °F
ASTM D1857
1540 °C
2800 °F
theoretical
Optical Properties Metric English Comments
Refractive Index 1.63
1.63
Component Elements Properties Metric English Comments
Al2O3 0.40 %
0.40 %
CaO 46.36 %
46.36 %
Fe2O3 0.77 %
0.77 %
K2O 0.020 %
0.020 %
Loss on Ignition(%) 0.50 %
0.50 %
MgO 0.15 %
0.15 %
MnO 0.15 %
0.15 %
SiO2 51.6 %
51.6 %
TiO2 0.050 %
0.050 %
Electrical Properties Metric English Comments
Electrical Resistivity 1.30e+13 ohm-cm
1.30e+13 ohm-cm
pure wollastonite
Dielectric Constant 6.8
<br>@Frequency 10000 Hz
6.8
<br>@Frequency 10000 Hz
6.8
<br>@Frequency 100000 Hz
6.8
<br>@Frequency 100000 Hz
6.9
<br>@Frequency 1.00e+6 Hz
6.9
<br>@Frequency 1.00e+6 Hz
6.9
<br>@Frequency 1000 Hz
6.9
<br>@Frequency 1000 Hz
Dissipation Factor 0.00152
<br>@Frequency 1000 Hz
0.00152
<br>@Frequency 1000 Hz
0.0046
<br>@Frequency 10000 Hz
0.0046
<br>@Frequency 10000 Hz
0.0046
<br>@Frequency 1.00e+6 Hz
0.0046
<br>@Frequency 1.00e+6 Hz
0.0078
<br>@Frequency 100000 Hz
0.0078
<br>@Frequency 100000 Hz
Descriptive Properties Value Comments
Appearance White
Bulking Value (gal./lbs.) 0.0413
Minus 325 U.S. Mesh Screen (%) 99.9
Morphology Acicular