Thermal Properties Metric English Comments
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
RT
Outokumpu 4016 Ferritic Stainless Steel
Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su..
Thermal Conductivity 25.0 W/m-K

@Temperature 400 °C
174 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4016 Ferritic Stainless Steel
Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su..
Thermal Conductivity 25.0 W/m-K

@Temperature 400 °C
174 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4021 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Thermal Conductivity 25.0 W/m-K

@Temperature 400 °C
174 BTU-in/hr-ft²-°F

@Temperature 752 °F
Outokumpu 4028 Martensitic Stainless Steel
Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat..
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 155 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy
This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm..
Thermal Conductivity 25.1 W/m-K
174 BTU-in/hr-ft²-°F
Misumi G-STAR Martensite Free-cutting Stainless Steel
Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation.
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 12 Lead Solder Alloy
Tin-free indium solderInformation Provided by Indium Corporation
Thermal Conductivity 25.0 W/m-K

@Temperature 85.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy
High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment)
Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g..
Thermal Conductivity 25.1 W/m-K

@Temperature 20.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Schmolz + Bickenbach 416RS Stainless Steel Bar
Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
CoorsTek StatSafe™ ADC Static Dissipative Alumina
Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes..
Thermal Conductivity 25.1 W/m-K

@Temperature 100 °C
174 BTU-in/hr-ft²-°F

@Temperature 212 °F
Crucible Steel 422 Stainless Steel
Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
China-Yixing Longly Refractories ZTA (10%ZrO2) Zirconia Toughened Alumina Composite Ceramic
LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir..
Thermal Conductivity 25.1 W/m-K
174 BTU-in/hr-ft²-°F
hardened to 45 HRC
Bohler-Uddeholm ORVAR® 2M / AISI H13 Hot Work Tool Steel
Orvar 2 Microdized is a chromium-molybdenum-vanadium alloyed steelORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hard..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
perpendicular
Carlisle 201HD Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 - 100 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Anderman Ceramics EC90P Mullite-Bonded Porous Silicon Carbide (90%)
Excellent thermal shock properties and thermal conductivity when in contact with molten metal. Available as tube, sheath, or rod up to 6 ft (1.9 m) long with diameters 0.6" to 3.75".Information pro..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 16.4% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 2.9% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 34.5% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 20% Cold Work
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 - 100 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Anderman Ceramics EA995 Sintered Alumina, 99.5%
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
Ceradyne Ceralloy® 225 Titanium Diboride
Features:electrical conductancewear resistancehardnessApplications:wear componentsballistic armorsputtering targetsInformation provided by Ceradyne Company
Thermal Conductivity 25.0 W/m-K
174 BTU-in/hr-ft²-°F
409 HP™
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel
AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze..
Thermal Conductivity >= 25.0 W/m-K
>= 174 BTU-in/hr-ft²-°F
Advanced Ceramics ACL 1091 (C-799) Alumina
Information provided by Advanced Ceramics Limited (ACL)
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment)
Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g..
Copyright © lookpolymers.com All Rights Reserved