Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.154 W/m-K | 1.07 BTU-in/hr-ft²-°F | ASTM D2214 |
Lord Adhesives Thermosetâ„¢ SC-300M Silicone Gel Encapsulant SC-300M is a two-part, rapid curing, platinum-catalyzed, addition cured, silicone gel. It has an extremely soft, gel-like consistency when cured, and has excellent unprimed adhesion to most substrat.. |
|||
Thermal Conductivity | 0.154 W/m-K | 1.07 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® T85 Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 131°Chigh impact and notched impact strengthPreprocessingMax. Water content |
|||
Thermal Conductivity | 0.154 W/m-K | 1.07 BTU-in/hr-ft²-°F | Melt |
Covestro Bayblend® T85 XF Polycarbonate + ABS General purpose injection molding gradeVicat/B 120 temperature = 130°Cbetter flow than T85PreprocessingMax. Water content |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
|
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 1200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 142 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 200 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 75 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.154 W/m-K @Temperature 100 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Dow SPECFLEX™ NC 630 Polyol SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082.. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 100 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt.. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 300 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 400 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 500 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.155 W/m-K @Temperature 25.0 - 75.0 °C |
1.07 BTU-in/hr-ft²-°F @Temperature 77.0 - 167 °F |
(Mylar® 1000A) |
DuPont Teijin Films Mylar® A Polyester Film, 92 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
Thermal Conductivity | 0.154 W/m-K @Thickness 6.35 mm, Temperature 44.3 °C |
1.07 BTU-in/hr-ft²-°F @Thickness 0.250 in, Temperature 112 °F |
|
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |