Polymer Property : Thermal Conductivity = 0.451 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT135 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT170 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT270 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT55 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT80 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Liquid
3M Fluorinert™ FC-40 Electronic Liquid
3M™ Fluorinert™ Liquid FC-40 is a non-conductive, thermally and chemically stable fluid ideal for single phase heat transfer fluid applications, especially in the electronics and semiconductor ind..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Liquid
3M Fluorinert™ FC-43 Electronic Liquid
3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct..
Thermal Conductivity 0.0650 W/m-K
0.451 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HT110 PFPE Heat Transfer Fluid
Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service tem..