Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | ASTM C158 |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52616 |
Parabeam Industrie Paraglass 3 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52616 |
Parabeam Industrie Paraglass 5 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklay one-step process a lightweight and strong sandwich laminate is formed that offers excellent mechan.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52616 |
Parabeam Industrie Paraglass 8 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52616 |
Parabeam Industrie ParaTank 4.5 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52616 |
Parabeam Industrie ParaTank 6 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Thermal Conductivity | 0.0600 - 7.10 W/m-K | 0.416 - 49.3 BTU-in/hr-ft²-°F | Average value: 0.844 W/m-K Grade Count:60 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Thermal Conductivity | 0.0600 - 0.120 W/m-K | 0.416 - 0.833 BTU-in/hr-ft²-°F | Average value: 0.0851 W/m-K Grade Count:6 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Thermal Conductivity | 0.0600 - 32.0 W/m-K | 0.416 - 222 BTU-in/hr-ft²-°F | Average value: 1.64 W/m-K Grade Count:35 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Thermal Conductivity | 0.0600 - 6.50 W/m-K | 0.416 - 45.1 BTU-in/hr-ft²-°F | Average value: 1.09 W/m-K Grade Count:59 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | |
MarkeTech Resorcinol Formaldehyde Aerogel Monolithic resorcinol formaldehyde (RF) nanofoams are primarily used as the precursor for carbon nanofoams or when an organic, electrically insulating material is desired. The standard RF nanofoam i.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV5813 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV5818 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV5810 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52 612 |
Brandenburger BRA-FLEX Side Insulation Information provided by Brandenburger Isoliertechnik GmbH&Co. |
|||
Thermal Conductivity | 0.0600 - 0.160 W/m-K | 0.416 - 1.11 BTU-in/hr-ft²-°F | |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Thermal Conductivity | 0.0600 - 0.160 W/m-K | 0.416 - 1.11 BTU-in/hr-ft²-°F | |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Thermal Conductivity | 0.0600 W/m-K @Temperature 200 °C |
0.416 BTU-in/hr-ft²-°F @Temperature 392 °F |
Arlon SQA-TMS-022 |
Arlon 680-R3839R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub.. |
|||
Thermal Conductivity | 0.0600 - 0.160 W/m-K | 0.416 - 1.11 BTU-in/hr-ft²-°F | |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Thermal Conductivity | 0.0600 - 0.160 W/m-K | 0.416 - 1.11 BTU-in/hr-ft²-°F | |
3M H50/10000EPX Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Thermal Conductivity | 0.0600 - 0.160 W/m-K | 0.416 - 1.11 BTU-in/hr-ft²-°F | |
3M D32/4500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | |
3M Novec™ 774 Engineered Fluid 3M™ Novec™ 774 Engineered Fluid is a clear, colorless and low odor fluid, and is one in a line of 3M products designed as replacements for ozone depleting substances (ODSs) and compounds with high.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | |
Goodfellow Cellophane, Rayophane Regenerated Cellulose Fiber All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | Fiber |
Goodfellow Cellophane, Rayophane Regenerated Cellulose Film All forms of cellulose degrade before they melt but natural cellulose can be regenerated by the xanthate process to manufacture fibres, commonly called rayon or viscose, and film, commonly called by.. |
|||
Thermal Conductivity | 0.0600 W/m-K | 0.416 BTU-in/hr-ft²-°F | DIN 52616 |
Parabeam Industrie ParaTank 3 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |