Thermal Properties Metric English Comments
Thermal Conductivity 50.0 - 200 W/m-K
347 - 1390 BTU-in/hr-ft²-°F
NanoAmor 50% Regular Single Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, and gas-discharge tubes in telecom networksElectromagnetic-wave absorption an..
Thermal Conductivity 50.0 - 200 W/m-K
347 - 1390 BTU-in/hr-ft²-°F
NanoAmor 95%, OD/ID: 20-40/5-10 nm Aligned Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Thermal Conductivity 50.0 W/m-K

@Temperature 85.0 °C
347 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy
Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 50.0 W/m-K

@Temperature 85.0 °C
347 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy
Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 50.0 W/m-K

@Temperature 85.0 °C
347 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy
Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation
Thermal Conductivity 50.0 W/m-K
347 BTU-in/hr-ft²-°F
ASTM E1461
M Cubed Technologies RBBC-751 Reaction Bonded Boron Carbide
Reaction-bonded boron carbide for extreme wear environments. Can be cast into very large components (greater than 4 ft. square)Information provided by M Cubed Technologies, Inc.
Thermal Conductivity 50.0 - 100 W/m-K
347 - 694 BTU-in/hr-ft²-°F
Perpendicular to Plane
Goodfellow Carbon-Carbon Composite
Carbon Fiber - Carbon MatrixInformation provided by Goodfellow.
Thermal Conductivity 50.0 - 75.0 W/m-K
347 - 521 BTU-in/hr-ft²-°F
Goodfellow Phosphor Bronze
Good Machinability. Uses include springs, clips, gauzes and architectural applicationsInformation provided by Goodfellow.
Thermal Conductivity 50.0 W/m-K
347 BTU-in/hr-ft²-°F
ASTM-C408
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide
Lowest density for ultra-lightweight designs
Thermal Conductivity 50.0 W/m-K
347 BTU-in/hr-ft²-°F
in plane
Carlisle 201HL Carbon-Carbon Composite
Carbon-Carbon Composite manufactured as sheets from 4mm to 125mm thick this material is essentially a fracture tough, fiber reinforced graphite often referred to as a “CFC”. Good for use in air t..