Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.540 W/m-K | 3.75 BTU-in/hr-ft²-°F | X-Y; ASTM E1461 |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Thermal Conductivity | 0.540 W/m-K | 3.75 BTU-in/hr-ft²-°F | |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Thermal Conductivity | 0.540 W/m-K | 3.75 BTU-in/hr-ft²-°F | |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Thermal Conductivity | 0.540 - 0.580 W/m-K | 3.75 - 4.03 BTU-in/hr-ft²-°F | Average value: 0.560 W/m-K Grade Count:3 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Thermal Conductivity | 0.540 W/m-K | 3.75 BTU-in/hr-ft²-°F | ASTM C518 |
Sumitomo Bakelite North America RX® 525 Cellulose Reinforced Phenolic Novolac RX 525 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for parts requiring moderate toughness. It is designed to meet the requirements of ASTM D-594.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 4466 Phenolic, Granular, Injection Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 4300 Phenolic, Granular, Compression Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 6301 Phenolic, Granular, Injection Molded PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 100 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1461 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Thermal Conductivity | 0.540 W/m-K | 3.75 BTU-in/hr-ft²-°F | ASTM C518 |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |
|||
Thermal Conductivity | 0.540 - 0.540 W/m-K @Temperature 100 - 100 °C |
3.75 - 3.75 BTU-in/hr-ft²-°F @Temperature 212 - 212 °F |
Average value: 0.540 W/m-K Grade Count:2 |
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi.. |
|||
Thermal Conductivity | 0.540 W/m-K @Temperature 25.0 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Mateck Thallium Bromoiodide TIBr-TII (KRS-5) Optical crystals |