Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.371 g/cc | 0.2663 lb/in³ | |
Solubility | 0.050 ppm | 0.050 ppm | |
a Lattice Constant | 0.4125 Å | 0.4125 Å |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Vickers Microhardness | 350 | 350 | MPa |
Modulus of Elasticity | 31.0 GPa | 4500 ksi | |
Poissons Ratio | 0.37 | 0.37 | |
Shear Modulus | 12.0 GPa | 1740 ksi |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.00 µm/m-°C @Temperature 20.0 °C |
3.33 µin/in-°F @Temperature 68.0 °F |
|
Specific Heat Capacity | 0.151 J/g-°C | 0.0361 BTU/lb-°F | |
Thermal Conductivity | 0.540 W/m-K @Temperature 25.0 °C |
3.75 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Melting Point | 414.5 °C | 778.1 °F |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 2.37 | 2.37 | at n10.0 |
2.21 @Wavelength 40000 nm |
2.21 @Wavelength 40000 nm |
||
2.29 @Wavelength 30000 nm |
2.29 @Wavelength 30000 nm |
||
2.38 @Wavelength 4000 nm |
2.38 @Wavelength 4000 nm |
||
2.60 @Wavelength 600 nm |
2.60 @Wavelength 600 nm |
||
Transmission, Visible | 10 % @Wavelength 650 nm |
10 % @Wavelength 650 nm |
Internal Transmittance |
70 % @Wavelength 670 nm |
70 % @Wavelength 670 nm |
Internal Transmittance | |
IR Transmittance | 10 % @Wavelength 50000 nm |
10 % @Wavelength 50000 nm |
Internal Transmittance |
72 % @Wavelength 25000 nm |
72 % @Wavelength 25000 nm |
Internal Transmittance |
Descriptive Properties | Value | Comments |
---|---|---|
Symmetry Class | m3m Pm3m | |
Syngony | cubic | |
Transmission Range (microns) | 0.6 - 40 |