Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:G.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM D1269E |
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC
(discontinued **) Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Thermal Conductivity | 0.300 - 0.548 W/m-K | 2.08 - 3.80 BTU-in/hr-ft²-°F | Average value: 0.424 W/m-K Grade Count:4 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Thermal Conductivity | 0.300 - 0.504 W/m-K | 2.08 - 3.50 BTU-in/hr-ft²-°F | Average value: 0.422 W/m-K Grade Count:11 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP Thermotuf VF002 PA 66 LNP THERMOTUF* VF002 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas region. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 121 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 250 °F |
|
Tra-Con Tra-Bond 293-1 General Purpose Instrument Epoxy Adhesive TRA-BOND 293-1 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293-se.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | ASTM E1461 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | Dry |
Asahi Kasei Leona® 14G25 25% Glass Filled Nylon 66 Enhanced strength and stiffness; with 25% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Thermal Conductivity | 0.300 - 0.401 W/m-K | 2.08 - 2.78 BTU-in/hr-ft²-°F | ASTM E1461-92 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | |
Chevron Phillips Ryton® PR09-60 Polyphenylene Sulfide Compound
(discontinued **) Polyphenylene Sulfide CompoundRyton® PR09-60 is pelletized unfilled high molecular weight polyphenylene sulfide resin suitable for extrusion or injection molding.Comments: Test specimen molding con.. |
|||
Thermal Conductivity | 0.300 W/m-K | 2.08 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |