Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | |
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem.. |
|||
CTE, linear | 130 - 160 µm/m-°C @Temperature 20.0 °C |
72.2 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
CTE, linear | 130 - 150 µm/m-°C @Temperature 20.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
CTE, linear | 130 - 160 µm/m-°C @Temperature 20.0 °C |
72.2 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | Above Tg |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | Above Tg |
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p.. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | Above Tg |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® K200 Standard Grade Acetal Resin Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® K500 Standard Grade Acetal Resin General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® K900 Standard Grade Acetal Resin Very low viscosity grade. Applications: Thin and large products.Information provided by API-Kolon. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 - 100 °C |
72.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 - 100 °C |
72.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® TD-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond F175 One-Part UV Curing Adhesive TRA-BOND F175 is a clear, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure with ult.. |
|||
CTE, linear | 130 µm/m-°C @Temperature -30.0 - 100 °C |
72.2 µin/in-°F @Temperature -22.0 - 212 °F |
|
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Glass Fluon® P-65P PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M25-44/M25S Acetal Co-polymer (POM), Standard, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 - 100 °C |
72.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |