Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 110 - 130 µm/m-°C @Temperature 100 - 100 °C |
61.1 - 72.2 µin/in-°F @Temperature 212 - 212 °F |
Average value: 120 µm/m-°C Grade Count:3 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | Above Tg |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
CTE, linear | 110 - 120 µm/m-°C | 61.1 - 66.7 µin/in-°F | ASTM D696 |
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide PTFE G Standard Compound with molybdenum disulphite. Enhanced non-stick properties. Low static coefficient of friction. Fairly good resistance to deformation. Applications: Guide bands. Details ne.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 285E3720005 Butyrate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307A4000015 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 307A4000018 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360A4861316 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 360E2R30016 Cellulose Acetate Propionate, Natural, Trsp Applications:AppliancesPersonal Care and CosmeticsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 360E3V45516 Propionate Water Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C @Temperature 20.0 °C |
61.1 - 94.4 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite 380A3V32818 Propionate Clear, Trsp Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties if Tenite cellulosi.. |
|||
CTE, linear | 110 - 170 µm/m-°C | 61.1 - 94.4 µin/in-°F | ASTM D696 |
Eastman Tenite 383A4000011 Cellulose Acetate Propionate, Clear, Trsp Applications:AppliancesFloor carePersonal care and cosmeticsProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, stren.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® 110-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 20.0 °C |
61.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 110 µm/m-°C @Temperature 25.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 77.0 - 131 °F |
ASTM E831 |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® EB-08 Acetal Co-polymer (POM), Conductive, Antistatic DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C | 61.1 µin/in-°F | DIN 52328 |
Isoflon PA 11 Polyamide 11 General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® HP270X Acetal Co-polymer (POM), High stiffness, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 110 µm/m-°C @Temperature 23.0 - 55.0 °C |
61.1 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M270-48 Acetal Co-polymer (POM), Antistatic, High flow DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |