Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 58.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 105 µm/m-°C

@Temperature 23.0 - 100 °C
58.3 µin/in-°F

@Temperature 73.4 - 212 °F
Quadrant EPP Ertalon® 6 SA PA 6, extruded (ISO Data)
This material offers an optimal combination of mechanical strength, stiffness, toughness, mechanical damping properties and wear resistance. These properties, together with good electrical insulatin..
CTE, linear 105 µm/m-°C
58.3 µin/in-°F
Above Tg
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas ..
CTE, linear 105 µm/m-°C
58.3 µin/in-°F
ASTM D696
Manifattura Cattaneo PP H Polypropylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628..
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Arlon Thermabond® 51A50X020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 76..
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E831
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate
Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico..
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 100 °C
58.3 µin/in-°F

@Temperature 68.0 - 212 °F
3M Scotch-Weld™ DP805 Acrylic Adhesives
3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability ..
CTE, linear 105 µm/m-°C

@Temperature -30.0 - 80.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel..
CTE, linear 105 µm/m-°C

@Temperature -30.0 - 80.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay E..
CTE, linear 105 µm/m-°C

@Temperature -30.0 - 80.0 °C
58.3 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228
Solvay Engineered Polymers DEXPRO® R116 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R116 is a thermoplastic polyolefin elastomeric. It is unfilled, reactor-grade molding compound. Applications: Exterior trim Information provided by Solvay Engineered Polymers..
CTE, linear 105 µm/m-°C

@Temperature 20.0 - 160 °C
58.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber
Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib..