Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 °C |
5.72 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Silicon Carbide (6H) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 3.5%. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 °C |
5.72 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Strontium Titanate (SrTiO3) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 °C |
5.72 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 25.0 - 600 °C |
5.72 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE ZrO Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 100 °C |
5.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
Misumi G-STAR Martensite Free-cutting Stainless Steel Corrosion resistant; excellent machinability. Comparable in material properties and chemical make up to STAVAX mold steel.Information provided by MISUMI Corporation. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 100 °C |
5.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 263 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability an.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 °C |
5.72 µin/in-°F @Temperature 68.0 °F |
|
Sapco Partially Stabilized TZP Zirconia (YSZ) Information provided by Sapco. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 25.0 - 1000 °C |
5.72 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek Yttria Partially Stabilized Zirconia, YZTP, Sintered Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 25.0 - 1000 °C |
5.72 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
CTE, linear | 10.3 µm/m-°C | 5.72 µin/in-°F | |
Anderman Ceramics EZY 94 Zirconia, 94%, Yttria-Stabilized Dense impervious zirconia for high wear and aggressive engineering applications. Available in many shapes and sizes.Information provided by Anderman Ceramics. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 25.0 - 1000 °C |
5.72 µin/in-°F @Temperature 77.0 - 1830 °F |
|
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |
|||
CTE, linear | 10.3 µm/m-°C | 5.72 µin/in-°F | |
Mateck YSZ Substrate bicrystals for superconductivity |