| Category | Ceramic , Oxide , Zirconium Oxide |
| Manufacturer | Sapco |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Sapco Partially Stabilized TZP Zirconia (YSZ).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 6.05 g/cc | 0.219 lb/in³ | |
| Open Porosity | 0.00 % | 0.00 % | |
| Weibull Modulus | 22 | 22 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Mohs | 8.0 | 8.0 | |
| Modulus of Elasticity | 200 GPa | 29000 ksi | |
| Flexural Strength | 1000 MPa | 145000 psi | |
| Compressive Strength | 2100 MPa | 305000 psi | |
| Poissons Ratio | 0.31 | 0.31 | |
| Shear Modulus | 76.0 GPa | 11000 ksi | Calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.3 µm/m-°C @Temperature 20.0 °C |
5.72 µin/in-°F @Temperature 68.0 °F |
|
| Specific Heat Capacity | 0.400 J/g-°C | 0.0956 BTU/lb-°F | |
| Thermal Conductivity | 2.00 W/m-K | 13.9 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 1100 °C | 2010 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 1.00e+9 ohm-cm | 1.00e+9 ohm-cm |