Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco 400 WOLLASTOCOAT® Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco ASPECT® 4000 Wollastonite ASPECT 4000 is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive .. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco HARRP™ 40 Wollastonite HARRP™ 40 is suggested for concrete, roof tile, grout/stucco, etc. reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distin.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco HARRP™ Coarse Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M1250 AS WOLLASTOCOAT® Wollastonite Chemically treated grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal per.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M1250 ES WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M200 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco M3 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco MD1250 WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco MG WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD G® WOLLASTOCOAT® Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® 5000 Wollastonite Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® G Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYAD® MD200 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYCOR® 100 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYCOR® R Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® 4W Wollastonite High aspect ratio grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctiv.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M15 Wollastonite High aspect ratio grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal perf.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M3 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco NYGLOS® M30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 1000 °C |
3.61 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories H-1 High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 6.50 - 7.10 µm/m-°C @Temperature 20.0 - 1000 °C |
3.61 - 3.94 µin/in-°F @Temperature 68.0 - 1830 °F |
|
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 200 °C |
3.61 µin/in-°F @Temperature 68.0 - 392 °F |
hardened to 62 HRC |
Bohler-Uddeholm AISI A2 Cold Work Tool Steel Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c.. |
|||
CTE, linear | 6.50 - 7.80 µm/m-°C @Temperature 25.0 - 800 °C |
3.61 - 4.33 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 95 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco ULTRAFIBRE® 30 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C | 3.61 µin/in-°F | |
Nyco ULTRAFIBRE® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -60.0 - 60.0 °C |
3.61 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Zinc Sulfide Cleartran (ZnS) Optical Crystals |