Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 41.0 - 88.0 µm/m-°C @Temperature 50.0 - 300 °C |
22.8 - 48.9 µin/in-°F @Temperature 122 - 572 °F |
Average value: 61.0 µm/m-°C Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
CTE, linear | 41.0 µm/m-°C @Temperature -30.0 - 100 °C |
22.8 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ RTA3263EUV Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV fractional melt flow, 1,500 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent com.. |
|||
CTE, linear | 41.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
D696 |
Zhejiang Juner 301-G10 10% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
CTE, linear | 41.0 µm/m-°C | 22.8 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
CTE, linear | 41.0 µm/m-°C | 22.8 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy Product Description: EPO-TEK® OG116-31 is a single component, UV curable epoxy adhesive and encapsulant, designed for PCB and circuit assembly applications found in semiconductor, computer, medical.. |
|||
CTE, linear | 41.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
22.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Beijing Chemical Industry KAIFA® 301-G10 PBT Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |