Polymer Property : CTE, linear = 0.833 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 1.50 - 80.0 µm/m-°C
0.833 - 44.4 µin/in-°F
Average value: 23.9 µm/m-°C Grade Count:23
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
CTE, linear 1.50 µm/m-°C
0.833 µin/in-°F
at Set Pt.
Ferro EG 0225 Specialty Glass
Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri..
CTE, linear 1.50 - 1.80 µm/m-°C
0.833 - 1.00 µin/in-°F
MarkeTech H-2 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
CTE, linear 1.50 - 1.80 µm/m-°C
0.833 - 1.00 µin/in-°F
MarkeTech H-3 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
CTE, linear 1.50 - 1.80 µm/m-°C
0.833 - 1.00 µin/in-°F
MarkeTech H-4 Honeycomb Ceramic
MarkeTech International special honeycomb ceramics have a uniform lattice structure, low expansion coefficient, good thermal shock resistance, higher specific surface area, low-pressure drop, and lo..
CTE, linear 1.50 µm/m-°C

@Temperature 0.000 - 70.0 °C
0.833 µin/in-°F

@Temperature 32.0 - 158 °F
DIN 53752
Borealis Beta-PPR™ RA7050 Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050 is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof of t..
CTE, linear 1.50 µm/m-°C

@Temperature 0.000 - 70.0 °C
0.833 µin/in-°F

@Temperature 32.0 - 158 °F
DIN 53752
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o..
CTE, linear 1.50 µm/m-°C
0.833 µin/in-°F
Cured
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating
AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of..
CTE, linear 1.50 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
0.833 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
CTE, linear 1.50 - 198 µm/m-°C
0.833 - 110 µin/in-°F
Average value: 106 µm/m-°C Grade Count:14
Overview of materials for Polypropylene, Extrusion Grade