Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 64.8 - 81.0 µm/m-°C | 36.0 - 45.0 µin/in-°F | Average value: 71.6 µm/m-°C Grade Count:5 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Styron EMERGEâ„¢ 8600-10 Polycarbonate EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental .. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 893-10 Polycarbonate CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 893-20 Polycarbonate CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
36.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron EMERGEâ„¢ 4800-7 Polycarbonate EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature -30.0 - 30.0 °C |
36.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D-3386 |
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7450 Rigid PVC, Extrusion Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7456 Rigid PVC, Extrusion Georgia Gulf 7456 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessWeatherabilityWeldabilityChemical ResistanceEase of Proces.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 5055 Rigid PVC, Extrusion, White Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7055 Rigid PVC, Extrusion Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7555 Rigid PVC, Extrusion, Natural Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7555 Rigid PVC, Extrusion, White Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7765 Rigid PVC, Extrusion Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7768 Rigid PVC, Extrusion Georgia Gulf 7768 is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityDimen.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-9900-0576 Unreinforced, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 5006 Rigid PVC, Extrusion, Natural Georgia Gulf 5006 Natural is a rigid PVC pellet compound designed for extrusion of interior rigid PVC profiles and various contours where high gloss and ease of processing is required. Georgia Gulf.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 5006 Rigid PVC, Extrusion, White Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia G.. |
|||
CTE, linear | 64.8 µm/m-°C @Temperature 20.0 °C |
36.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 5055 Rigid PVC, Extrusion, Natural Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p.. |