Polymer Property : CTE, linear = 52.2 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 52.2 µm/m-°C

@Temperature -18.0 - 38.0 °C
29.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Plaskolite Optix® Acrylic Sheet
Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,..
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
ASTM D696
Quantum PPS
Information provided by Quantum Advanced Engineering Plastics
CTE, linear 52.2 µm/m-°C

@Temperature 20.0 °C
29.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum
Information provided by ITW Devcon
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
Ensinger Hydel® PEI-7 Polyetherimide (PEI), Static Dissipative
A static dissipative polyetherimide utilizing proprietary filler technology which renders this material electrically conductive. This technology allows for good dimensional stability after machinin..
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
ASTM D696
Ensinger PVC Polyvinylchloride (PVC)
Ensinger's type 1 grey PVC ROD is designed for machining solutions and is a cost effective solution for general industrial applications. The material offers an excellent combination of chemical resi..
CTE, linear 52.2 µm/m-°C
29.0 µin/in-°F
BCC Products MB 3500 Urethane Fixture Board
MB 3500 is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly sha..
CTE, linear 52.2 - 100 µm/m-°C
29.0 - 55.6 µin/in-°F
Average value: 70.1 µm/m-°C Grade Count:4
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
CTE, linear 52.2 - 101 µm/m-°C
29.0 - 56.0 µin/in-°F
Average value: 75.7 µm/m-°C Grade Count:14
Overview of materials for Acrylic, Optical Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr..