Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.40 - 63.0 µm/m-°C | 3.00 - 35.0 µin/in-°F | Average value: 37.7 µm/m-°C Grade Count:59 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 400 °C |
3.00 µin/in-°F @Temperature 68.0 - 752 °F |
|
Hogen HM1000 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offe.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 1000 °C |
3.00 µin/in-°F @Temperature 68.0 - 1830 °F |
|
McDanel Advanced Ceramics MV-20 Mullite Information provided by McDanel Advanced Ceramic Technologies |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 1000 °C |
3.00 µin/in-°F @Temperature 68.0 - 1830 °F |
|
McDanel Advanced Ceramics MV-30 Mullite Information provided by McDanel Advanced Ceramic Technologies |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 400 °C |
3.00 µin/in-°F @Temperature 68.0 - 752 °F |
|
Mi-Tech Metals HD17 Tungsten-Based Metal Mil Spec T-21014D Class 1; ASTM B-777-99 Class 1; ASTM B-777-07 Class 1; SAE Aero Material Spec (AMS) 7725C; AMS T-21014 Class 1. Nil magnetic properties.Manufactured by powder metallurgy methods. .. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 400 °C |
3.00 µin/in-°F @Temperature 68.0 - 752 °F |
|
Mi-Tech Metals HD17BB Tungsten-Based Metal ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.00 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott DUROBAX® amber Neutral Glass Tubing Neutral glass tubing, chemically highly resistant, with light protection Containers, test tubes, pipettes, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, .. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 °C |
3.00 µin/in-°F @Temperature 68.0 °F |
|
SGL Carbon Group EK 2240 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 300 °C |
3.00 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott FIOLAX® amber Neutral Glass Tubing Neutral glass tubing, chemically highly resistant, with light protection Pharmaceutical primary packagingInformation provided by SCHOTT AG. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 °C |
3.00 µin/in-°F @Temperature 68.0 °F |
|
Zircar Ceramics AS-CEM Alumina-Silica Cement Type AS-CEM Alumina-Silica Cement is a high temperature resistant cement useful for creating a hard coating on the surfaces of ZIRCAR® Alumina-Silica fibrous ceramic products or other porous insula.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 1000 °C |
3.00 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SC40 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 20.0 - 1320 °C |
3.00 µin/in-°F @Temperature 68.0 - 2410 °F |
|
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
CTE, linear | 5.40 µm/m-°C | 3.00 µin/in-°F | |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 27.0 - 175 °C |
3.00 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 7957MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 27.0 - 175 °C |
3.00 µin/in-°F @Temperature 80.6 - 347 °F |
ASTM D696 |
3M 9057MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
CTE, linear | 5.40 µm/m-°C @Temperature 23.0 - 85.0 °C |
3.00 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |