| Category | Ceramic , Glass |
| Manufacturer | Schott North America |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Schott FIOLAX® amber Neutral Glass Tubing.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.42 g/cc <br>@Temperature 25.0 °C |
0.0874 lb/in³ <br>@Temperature 77.0 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 5.40 µm/m-°C <br>@Temperature 20.0 - 300 °C |
3.00 µin/in-°F <br>@Temperature 68.0 - 572 °F |
ISO 7991 |
| Transformation Temperature, Tg | 550 °C | 1020 °F | |
| Softening Point | 770 °C | 1420 °F | Viscosity 10<sup>7.6</sup> dPa s |
| Working Point | 1165 °C | 2129 °F | Viscosity 10<sup>4</sup> dPa s |
| Annealing Point | 560 °C | 1040 °F | Viscosity 10<sup>13</sup> dPa s |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 25 % <br>@Thickness 1.00 mm,<br> Wavelength 500 nm |
25 % <br>@Thickness 0.0394 in,<br> Wavelength 500 nm |
|
| 65 - 70 % <br>@Wavelength 650 - 800 nm,<br> Thickness 1.00 mm |
65 - 70 % <br>@Wavelength 650 - 800 nm,<br> Thickness 0.0394 in |
||
| 70 % <br>@Thickness 1.00 mm,<br> Wavelength 700 nm |
70 % <br>@Thickness 0.0394 in,<br> Wavelength 700 nm |
||
| IR Transmittance | 2.0 % <br>@Thickness 1.00 mm,<br> Wavelength 4700 nm |
2.0 % <br>@Thickness 0.0394 in,<br> Wavelength 4700 nm |
Cutoff |
| <= 30 % <br>@Wavelength >=3550 nm,<br> Thickness 1.00 mm |
<= 30 % <br>@Wavelength >=3550 nm,<br> Thickness 0.0394 in |
||
| 35 % <br>@Thickness 1.00 mm,<br> Wavelength 2800 nm |
35 % <br>@Thickness 0.0394 in,<br> Wavelength 2800 nm |
||
| 62 % <br>@Thickness 1.00 mm,<br> Wavelength 3300 nm |
62 % <br>@Thickness 0.0394 in,<br> Wavelength 3300 nm |
||
| 67 - 78 % <br>@Wavelength 800 - 1600 nm,<br> Thickness 1.00 mm |
67 - 78 % <br>@Wavelength 800 - 1600 nm,<br> Thickness 0.0394 in |
||
| 78 - 83 % <br>@Wavelength 1600 - 2650 nm,<br> Thickness 1.00 mm |
78 - 83 % <br>@Wavelength 1600 - 2650 nm,<br> Thickness 0.0394 in |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 6.0 % | 6.0 % | |
| B2O3 | 7.0 % | 7.0 % | |
| BaO | 2.0 % | 2.0 % | |
| CaO | <= 1.0 % | <= 1.0 % | |
| Fe2O3 | 1.0 % | 1.0 % | |
| K2O | 1.0 % | 1.0 % | |
| Na2O | 7.0 % | 7.0 % | |
| SiO2 | 70 % | 70 % | |
| TiO2 | 5.0 % | 5.0 % |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 1 | 1 | DIN 12116 |
| Alkali Class, AR | 2 | 2 | ISO 695 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Hydrolytic Resistance | Class HGB 1 | ISO 719 |
| fulfilled | JP | |
| Type I | Ph. Eur. | |
| Type I | USP |