Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 46.0 µm/m-°C @Temperature -30.0 - 100 °C |
25.6 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB285 high melt flow, 1,300 MPa flexural modulus, low CLTE, UV-stabilized, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of .. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
CTE, linear | 46.0 µm/m-°C | 25.6 µin/in-°F | ASTM D696 |
Unitika AXG-1500-300 Dry Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4466 Phenolic, Granular, Injection Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 20.0 °C |
25.6 µin/in-°F @Temperature 68.0 °F |
|
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 5488 Phenolic, Granular, Injection Molded PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not .. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4300 Phenolic, Granular, Injection Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4300 Phenolic, Granular, Transfer Molded PLENCO 04300 is a heat resistant, mineral filled phenolic molding compound offering optimum cure characteristics and excellent dimensional stability. It is formulated for wiring devices and electric.. |
|||
CTE, linear | 46.0 µm/m-°C | 25.6 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |
|||
CTE, linear | 46.0 µm/m-°C | 25.6 µin/in-°F | x direction |
Arlon IsoClad 917 Non-Woven Fiberglass Reinforced PTFE Traditional - Highest Performance, PTFE Coated Light Woven Glass Styles, Interdispersed PTFE FilmInformation provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 20.0 °C |
25.6 µin/in-°F @Temperature 68.0 °F |
|
Armstrong A-31 Epoxy Adhesive Is a neutral-colored thixotropic paste material having a creamy or buttery consistency that will not flow even when cured at elevated temperatures A-31 also features Extremely low outgassing charact.. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 20.0 °C |
25.6 µin/in-°F @Temperature 68.0 °F |
|
Armstrong A-40 Epoxy Adhesive Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re.. |
|||
CTE, linear | 46.0 µm/m-°C | 25.6 µin/in-°F | below Tg |
Gromax Evasin EV-3201V Ethylene-Vinyl Alcohol Copolymer Unmodified random Co-Polymer of [Ethylene-Vinyl alcohol], designed for therm-plastic processing into Sheets and Foils with high Oxygen and Aroma Barrier EffectInformation provided by Gromax Enterpri.. |
|||
CTE, linear | 46.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 7579 Phenolic, Granular, Injection Molded PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40.. |
|||
CTE, linear | 46.0 - 52.0 µm/m-°C @Temperature 40.0 - 130 °C |
25.6 - 28.9 µin/in-°F @Temperature 104 - 266 °F |
Average value: 48.0 µm/m-°C Grade Count:3 |