Polymer Property : CTE, linear = 198 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 198 µm/m-°C

@Temperature 20.0 °C
110 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet
Information provided by Röchling Engineered Plastics.
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 150 °C
110 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E831
Quadrant EPP Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 1000 UHMW-PE, Virgin (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW-PE, Natural & Colored Except Black (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f..
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C
110 µin/in-°F
ASTM E831
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet)
Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM..
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet)
CTE, linear 198 µm/m-°C

@Temperature 20.0 °C
110 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Rochling Engineered Plastics Polystone® P Polypropylene Extruded Sheet
Information provided by Röchling Engineered Plastics.
CTE, linear 198 µm/m-°C

@Temperature 20.0 °C
110 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Saint-Gobain Norton® UHMW PE Skived PTFE Film
Description: UHMWPE = ultra-high molecular weight polyethylene; PTFE = polytetrafluoroethyleneApplications include: Common in Protective/Decorative ApplicationsInformation provided by Saint Gobain P..
CTE, linear 198 µm/m-°C

@Temperature 20.0 °C
110 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Lennite® Ultra High Molecular Weight Polyethylene
Lennite UHMW-PE is a low friction engineering plastic with excellent chemical resistant and abrasive wear resistance. It is widely used in conveyors, packaging machinery, and food processing machin..
CTE, linear 198 µm/m-°C
110 µin/in-°F
Above Tg
Tra-Con Tra-Bond 526M04 Color Keyed High Temperature Epoxy Adhesive
TRA-BOND 526M04 is a low viscosity, high-temperature, two-part epoxy formulation with a long working life. TRA-BOND 526M04 exhibits excellent wicking, and develops strong, tough mechanically stable ..
CTE, linear 198 µm/m-°C

@Temperature -40.0 - 149 °C
110 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Quicksilver® UHMW-PE Premium Truck Lining (ASTM Product Data Sheet)