Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.930 g/cc | 0.930 g/cc | ASTM D792 |
Water Absorption | <= 0.010 % | <= 0.010 % | Immersion, 24hr; ASTM D570(2) |
Water Absorption at Saturation | <= 0.010 % | <= 0.010 % | Immersion; ASTM D570(2) |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 66 | 66 | ASTM D2240 |
Tensile Strength | 30.3 MPa | 4400 psi | ASTM D638 |
Elongation at Break | 230 % | 230 % | ASTM D638 |
Tensile Modulus | 0.483 GPa | 70.0 ksi | ASTM D638 |
Flexural Strength | 24.1 MPa | 3500 psi | ASTM D790 |
Flexural Modulus | 0.455 GPa | 66.0 ksi | ASTM D790 |
Compressive Strength | 20.7 MPa | 3000 psi | 10% Def.; ASTM D695 |
Compressive Modulus | 0.552 GPa | 80.0 ksi | ASTM D695 |
Shear Strength | 33.1 MPa | 4800 psi | ASTM D732 |
Izod Impact, Notched | NB | NB | ASTM D256 Type A |
Coefficient of Friction, Dynamic | 0.090 | 0.090 | Dry vs. Steel; QTM55007 |
Sand Slurry | 10 | 10 | 1018 Steel = 100; ASTM D4020 |
Limiting Pressure Velocity | 0.0701 MPa-m/sec | 2000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 198 µm/m-°C @Temperature -40.0 - 149 °C |
110 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Melting Point | 135 °C | 275 °F | Crystalline, Peak; ASTM D3418 |
Maximum Service Temperature, Air | 82.2 °C | 180 °F | Long Term |
Deflection Temperature at 1.8 MPa (264 psi) | 46.7 °C | 116 °F | ASTM D648 |
Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | ASTM D257 |
Dielectric Constant | 2.3 @Frequency 1e+6 Hz |
2.3 @Frequency 1e+6 Hz |
ASTM D150 |
Dielectric Strength | 90.0 kV/mm | 2290 kV/in | Short Term; ASTM D149 |
Dissipation Factor | <= 0.00050 @Frequency 1e+6 Hz |
<= 0.00050 @Frequency 1e+6 Hz |
ASTM D150 |
Compliance Properties | Metric | English | Comments |
---|---|---|---|
3A-Dairy | No | No | |
Canada AG | No | No | |
FDA | No | No | |
NSF | No | No | |
USDA | No | No | |
USP Class VI | No | No |
Chemical Resistance Properties | Metric | English | Comments |
---|---|---|---|
Acids, Strong (pH 1-3) | Limited | Limited | |
Acids, Weak | Acceptable | Acceptable | |
Alcohols | Acceptable | Acceptable | |
Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
Alkalies, Weak | Acceptable | Acceptable | |
Chlorinated Solvents | Acceptable | Acceptable | |
Conductive / Static Dissipative | No | No | |
Continuous Sunlight | Acceptable | Acceptable | |
Hot Water / Steam | Limited | Limited | |
Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
Inorganic Salt Solutions | Acceptable | Acceptable | |
Ketones, Esters | Limited | Limited |