Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 162 µm/m-°C @Temperature -40.0 - 149 °C |
90.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
CTE, linear | 162 - 216 µm/m-°C @Temperature 20.0 °C |
90.0 - 120 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
CTE, linear | 162 µm/m-°C @Temperature 20.0 °C |
90.0 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
CTE, linear | 162 µm/m-°C @Temperature 20.0 °C |
90.0 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ CC607 PTFE 35% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
CTE, linear | 162 µm/m-°C @Temperature 20.0 °C |
90.0 µin/in-°F @Temperature 68.0 °F |
|
3M Dyneon™ CC698 PTFE 20% Fiberglass/Carbon Filled
(discontinued **) Product Form: Black, pelletized powder. Applications include valve seats.Data provided by Dyneon. |
|||
CTE, linear | 162 µm/m-°C @Temperature 20.0 °C |
90.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Saint-Gobain Norton® ECTFE Fluoropolymer Film Features/Benefits:Outstanding release propertiesPerformance from -200°C (-328°F) to 165°C (330°F)High dielectric strengthExcellent chemical, radiation, weather and abrasion resistanceNon.. |
|||
CTE, linear | 162 µm/m-°C @Temperature 20.0 °C |
90.0 µin/in-°F @Temperature 68.0 °F |
|
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
CTE, linear | 162 µm/m-°C @Temperature -80.0 - -30.0 °C |
90.0 µin/in-°F @Temperature -112 - -22.0 °F |
ASTM D696 |
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
CTE, linear | 162 µm/m-°C | 90.0 µin/in-°F | |
BCC Products BC 100 Medium Cyanoacrylate Adhesive BC100 Medium, like its name in the medium viscosity version of cyanoacrylate adhesive that has become most popular in the super bonding applications. A 12 second fixture bond makes the BC100 the fas.. |
|||
CTE, linear | 162 µm/m-°C | 90.0 µin/in-°F | |
BCC Products BC 100 Thin Cyanoacrylate Adhesive BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas.. |
|||
CTE, linear | 162 µm/m-°C | 90.0 µin/in-°F | |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |
|||
CTE, linear | 162 - 216 µm/m-°C | 90.0 - 120 µin/in-°F | ASTM D696 |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |