Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Network Polymers Kepital® F20-03 Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Petromont 5000 High Density Polyethylene Resin Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa.. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | |
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated tem.. |
|||
CTE, linear | 130 µm/m-°C @Temperature -40.0 - 176 °C |
72.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 130 - 150 µm/m-°C @Temperature 20.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
CTE, linear | 130 - 160 µm/m-°C @Temperature 20.0 °C |
72.2 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | Above Tg |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® EL302 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Micropol Isoplas P471 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative) Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abra.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond F175T One-Part Thixotropic UV Curing Adhesive TRA-BOND F175T is a thixotropic, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure w.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® TD-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond F175 One-Part UV Curing Adhesive TRA-BOND F175 is a clear, one part UV curing adhesive designed for bonding metals, ceramics and most rigid polymers. It is an excellent adhesive for fiber optic terminations where fast cure with ult.. |
|||
CTE, linear | 130 - 150 µm/m-°C | 72.2 - 83.3 µin/in-°F | |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Glass Fluon® P-802UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® M25-44/M25S Acetal Co-polymer (POM), Standard, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 130 µm/m-°C @Temperature 20.0 - 100 °C |
72.2 µin/in-°F @Temperature 68.0 - 212 °F |
|
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® TD-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |