Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 °C |
6.60 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 °C |
6.60 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
CTE, linear | 11.9 µm/m-°C | 6.61 µin/in-°F | at Set Pt. |
Ferro EG 2760 Thick Film Glass Glass Type: Pb-B-Zn Typical Powder Form: MVG, VEG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduc.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 37.8 - 538 °C |
6.60 µin/in-°F @Temperature 100 - 1000 °F |
|
Meehanite GC-40 Flake Graphite Cast Iron Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 300 °C |
6.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott S8809 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 93.0 °C |
6.61 µin/in-°F @Temperature 199 °F |
|
Special Metals UDIMET® alloy 188 Cobalt-base Alloy UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small .. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 93.0 °C |
6.61 µin/in-°F @Temperature 199 °F |
|
Special Metals UDIMET® alloy R41 Ni-Cr Alloy UDIMET® alloy R41 (UNS N07041) is a precipitation-hardenable nickel-chromium alloy containing significant amounts of cobalt and molybdenum, along with lesser amounts of aluminum and titanium. Al.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 649 °C |
6.60 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 649 °C |
6.60 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 649 °C |
6.60 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 430 Ferritic Stainless Steel, Annealed Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 649 °C |
6.60 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 430 Ferritic Stainless Steel, Full Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 100 °C |
6.61 µin/in-°F @Temperature 68.0 - 212 °F |
|
AK Steel ASTM A 424 Type 1, UNIVIT® DS Enameling Carbon Steel UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling syst.. |
|||
CTE, linear | 11.9 µm/m-°C @Temperature 20.0 - 649 °C |
6.60 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Schmolz + Bickenbach IMRE™ Stainless Steel Bar Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand.. |