Thermal Properties | Metric | English | Comments |
---|---|---|---|
Softening Point | 80.0 °C | 176 °F | ISO 306 |
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene BL4M is a high density polyethylene with 1-Butene as co monomer. It is high molar mass, easily processable, high stiffness and strength, good SCR, very good molding surface finish.Applications: jer.. |
|||
Softening Point | 80.0 °C | 176 °F | ISO 306 |
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene EX2 is a high density polyethylene with 1-Butene as co monomer. It has good rigidity and medium molar mass. Applications: monofilaments, ropes, yarns.Information provided by Iran Petrochemical Com.. |
|||
Softening Point | 80.0 °C | 176 °F | ISO 306 |
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: .. |
|||
Softening Point | 80.0 - 85.0 °C | 176 - 185 °F | MQSA 70A |
Lubrizol Advanced Materials Pearlbond® D1160 Thermoplastic Polyurethane Pearlbond™ D1160 is a linear, aromatic polyurethane, supplied in form of small white granules, which combines a high crystallization rate and high thermoplasticity level. Applications: Pearlbo.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | |
Lucobit Lucobit® 1210A Ethylene Copolymer Bitumen Lucobit 1210A is a mixture of ethylene copolymers and special bitumen. Addition of Lucobit to bitumen increases its viscosity and broadens the range of plasticity.Lucobit 1210A in asphalt mixtures .. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | |
Lucobit Lucolast® 7010 Ethylene Butyl Acrylate Asphalt Additive Lucolast® 7010 is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Addition of Lucolast 7010 to bitumen increases its viscosity, broadens the range of plasticit.. |
|||
Softening Point | 80.0 °C | 176 °F | ISO 306 |
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene BL3VD is a high density polyethylene with 1-Butene as co monomer. It is very high density and stiffness, good ESCR, high flowability and impact strength.Applications: small blow molding, bottles, c.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 80.0 °C | 176 °F | |
Struktol VP 3735 Flame retarded epoxy resin Applications: STRUKTOL VP 3735 is a multifunctional epoxy resin, which contains a chemically bound organophosphorous substance. Thus the mechanical properties like tenacity and modulus are not influ.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-562 TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |
|||
Softening Point | 80.0 °C | 176 °F | JIS K-2531 |
Unitika elitel UE3300 Polyester, Flake Low molecular weight type UE3210, High OH type, Branched & highly crosslinkedUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications fro.. |
|||
Softening Point | 80.0 °C | 176 °F | |
Zeon Chemicals Quintone® N180 Aliphatic Hydrocarbon Resin C5/C9 type (piperylene and dicyclopentadiene precursor). Gives excellent tackiness to adhesives, especially suitable for hot-melt adhesives.Information provided by Zeon Chemicals L.P. |
|||
Softening Point | 80.0 - 100 °C | 176 - 212 °F | flow beginning |
Taiwan Sheen Soon Sheenthane® AH-560T TPU for Hotmelt Adhesive Thermoplastic polyurethane elastomer for soft hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes.. |