Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 165 °C | 104 - 329 °F | Average value: 56.3 °C Grade Count:20 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 55.0 - 165 °C | 131 - 329 °F | Average value: 145 °C Grade Count:11 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 125 - 165 °C | 257 - 329 °F | ISO 75-2 |
CENTROPLAST CENTROMID 12 soft Polyamide 12 soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 121 - 165 °C | 250 - 329 °F | Average value: 153 °C Grade Count:41 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |