Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 - 152 °C | 188 - 306 °F | Average value: 139 °C Grade Count:85 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | unannealed; ASTM D648 |
Styron Magnumâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) High Impact, High Heat, Blow Molding ABSInformation provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS LE WT Availability: North AmericaForms: PelletsFeatures: Low Extractables and Medium Impact ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Annealed; ASTM Data |
Dow Retain® PS-4000 Polystyrene Data provided by Dow Chemical. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | ASTM D648 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 86.7 °C | 188 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PP FR BK Availability: North AmericaForms: PelletsFeature: Flame Retardant, Homopolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |