Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**) Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ASTM D648 |
ExxonMobil Escorene® LL-8461 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good stiffnessUses: Septic tanks, Chemical storage bins, Potable water tanks |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ASTM D648 |
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C @Thickness 4.00 mm |
104 °F @Thickness 0.157 in |
after annealing 150°C 16 hr; ASTM D648 |
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer
(discontinued **) Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 135 °C | 104 - 275 °F | Average value: 67.5 °C Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ASTM D648 |
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | |
LATI Latigray 47/1-01 CX/45 PP Copolymer Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C @Thickness 3.20 mm |
104 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C @Thickness 3.20 mm |
104 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific) LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BRZ 247 W PA6 Product description: Grilon BRZ 247 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 247 W has the following important properties: High flexibi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® BRZ 347 W PA6 Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® XE 3841 nat PA12 Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 W 40 NZ PA12-I Product Description: Grilamid L 25 W 40 NZ is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 NZ is impact modified and heat and UV stabilized. The.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ASTM D648 |
Arkema Group PLATAMID® 8020 Copolyamide Platamid® 8020 is a transparent, thermoplastic copolyamide designed for conversion by standard molding or extrusion techniques.Information provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 55.0 °C | 104 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 55.0 °C | 104 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ISO 75-2 |
CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C @Thickness 4.00 mm |
104 °F @Thickness 0.157 in |
after annealing 150°C 16 hr; ASTM D648 |
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer
(discontinued **) Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | ASTM D648-07 |
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 °C | 104 °F | |
LATI Latiohm 52/11-10 PD02 PP Homopolymer Dissipative product based on Polypropylene homopolymer (PPh). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 98.9 °C | 104 - 210 °F | Average value: 77.5 °C Grade Count:54 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 40.0 - 55.0 °C | 104 - 131 °F | ASTM D648 |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |