Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Cycolac® S701S ABS (Europe-Africa-Middle East) CYCOLAC S701S is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appl.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | |
Polimeri Europa SINKRAL B620 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-25-20 High impact injection moulding grade. Its` excellent balance of mechanical properties (toughness -.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | |
Ineos ABS Lustran® 752 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
GRECO ISOPAK 540 ABS Resin Flame Retardant GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.35 mm |
174 °F @Thickness 0.250 in |
ASTM D648 |
IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | |
Ineos ABS Lustran® Elite HH 1827 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ISO 75-2 |
Kureha KF Polymer 1000 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 6.40 mm |
174 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C @Thickness 3.20 mm |
174 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 LNP* THERMOCOMP* RZ006S is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; 104°C (219°F) annealed; ASTM Data |
Styron Magnum™ 2610 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; 104°C (219°F) annealed; ASTM Data |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 800 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; 104°C (219°F) annealed; ASTM Data |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Unannealed; ASTM Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SC 202LV General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SP 554 Flame Retardant Polystyrene Characteristics Very good flow properties Good balance of toughness and rigidity Processing Molding Gas assist molding Applications Large size T.V. Cabinets VCR cabinets Electrical boxes, electr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SP6433 9710 Medium Impact Polystyrene Characteristics High flow Good toughness Good shine Available in various colors Processing Injection molding Extrusion Applications Pipes & profiles for wiring Beading for furniture and tables .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Supreme Petrochem SP6489 9940 High Impact Polystyrene Characteristics High flow Good toughness Available in black only Processing Injection moldingApplications TV and audio-video back and front cover Material Status: Commercial : ActiveAgency Ratings.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | unannealed; ISO 75 |
Chi Mei Polyrex® PH-888G Polystyrene - High gloss High impact; high gloss |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | 0.125";; ASTM D648 |
Diamond Polymers Centrex® 485 Sheet Extrusion Grade Centrex 485 resin is a low-gloss, medium-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 - 242 °C | 174 - 468 °F | Average value: 212 °C Grade Count:48 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 79.0 °C | 174 °F | ASTM D648 |
Ineos Nova 5504 High Impact Polystyrene