Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite Optix® CA - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
Plaskolite Optix® CA-990 Impact Modified Acrylic Resin Injection Molding and Extrusion Grade. Excellent surface gloss. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite Optix® CP - 927 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
Plaskolite West Optix® CA-990 Impact Modified Acrylic Resin Injection Molding and Extrusion Grade. Excellent surface gloss. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite West Optix® CP - 927 G High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite West Optix® CP - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 6.35 mm |
174 °F @Thickness 0.250 in |
unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS Acrylonitrile Butadiene Styrene, low gloss ABS.Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D-648 |
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
I. Stern GPPS-004 General Purpose Crystal Polystyrene Features:High Strength GradeMedium Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & C.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | TMA |
SABIC Innovative Plastics Valox® FR1 Polybutylene Terephthalate Film, Flame Retardant Valox FR-1 film is a flame retardant thermoplastic polybutylene, terephthalite film offering UL94 VTM-0 performance down to 125 microns and good temperature performance. Valox FR-1 film’s outst.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 6.35 mm |
174 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C @Thickness 6.35 mm |
174 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8002 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | ASTM D648 |
Lubrizol ESTALOC® 59600 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | 0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S210 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | 0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648 |
Diamond Polymers ASA S210B Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | |
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | |
Aclo Accucomp SAN SAN900L |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C | 174 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339M30L Mica Reinforced |