Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C @Thickness 3.18 mm |
151 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 161J1-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C @Thickness 6.35 mm |
151 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging M2288 Polyvinyl Chloride, Rigid (PVC, Rigid) Opaque sheet extrusion compound.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | Unannealed; ASTM D648 |
Multibase Nylex™ 2185 CR Polyamide + PP Forms: PelletsFeatures:Chemical Resistance, GoodInformation provided by Multibase |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C @Thickness 3.18 mm |
151 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging PK9 WHITE 1082 Polyvinyl Chloride, Rigid (PVC, Rigid) The HDT value refers to samples conditioned @ 50 deg.C. for 24 hrs.The bulk density test was performed under ASTM D-1895B.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 - 196 °C | 151 - 385 °F | Average value: 87.9 °C Grade Count:119 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | Unannealed; ISO 75A-1, -2 |
LyondellBasell Hostacomâ„¢ TKS709D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS709D medium high melt flow, 1,600 MPa flexural modulus, UV-stabilized, thermoplastic elastomeric olefin (TEO) resin has an excellent combination of properties and proc.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/10 BK Nylon 610 Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | unannealed (0.125 in); ASTM D648 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | |
Aclo Accuguard ABS ABS860V0L Flame Retardant |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | |
Aclo Accutech Polypropylene Copolymer CP0436W40L Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | |
Aclo Accutech Polypropylene Homopolymer HP0336W20L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | ASTM D-648 |
Axiall 7801 Rigid PVC, Extrusion, White, High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | ASTM D-648 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 66.1 °C | 151 °F | unannealed; ASTM D-648 |
Axiall 8607 Rigid PVC, Extrusion Georgia Gulf 8607 is a special purpose pelletized compound formulated for high impact, rigid extrusion profiles.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |